WGL
White gold solder for furnace soldering after firing BEGO cobalt-chrome and BEGO nickel-chrome metal-to-ceramic alloys.

CE 0197
Melting interval: 770-730 ºC, soldering temperature: 860 ºC, Flux: Minoxyd.
Technical data Alloy characteristics Composition in % by weight
| |||||||||||||